Product Selection Guide

Match the application to the material. Every product below is listed with its key mechanical value and the standard it is tested to, so the choice can be checked rather than assumed.

1. Choose by application

ApplicationRecommended productKey valueStandardWhy this one
Bridge bearing installationH60 Bearing Grouting Materialβ‰₯60 MPa (25℃ curing)JC/T 986-2018High-flow, non-shrink grout for bearing seats and structural support
Equipment and machine basesHigh Strength Non-Shrink Grouting Material1d β‰₯20 MPa / 3d β‰₯40 MPa / 28d β‰₯60 MPaGB/T 50448-2015Load transfer under base plates and anchor bolts
Precast concrete connectionsSleeve Grouting Materialβ‰₯85 MPaJG/T 408-2019Rebar splicing in sleeves, tested to JG/T 408
Wind turbine foundationsWind Turbine Foundation Grouting Material>100 MPaGB/T 50448‑2015Tower-to-foundation connections, onshore and offshore
Tunnel vault and backfillTunnel Vault Grouting Materialβ‰₯60 MPaGB/T 50448‑2015Void filling and lining contact grouting
Prestressed duct groutingPrestressed Duct Grouting Material3d β‰₯20 MPa / 7d β‰₯40 MPa / 28d β‰₯50 MPaJTG/T F50-2011Duct filling with low bleed and volume stability
Underwater repairUnderwater Non-Dispersible Grouting Material50–90 MPa (depending on class)GB/T 50448‑2015Non-dispersible grout placed in water
Cement pavement repairCement Pavement Repair Material1d β‰₯25 MPa / 3d β‰₯40 MPa / 28d β‰₯50 MPaJT/T 1124-2017Rapid opening to traffic, thin-layer patching
Rebar anchoring / plantingRebar Anchoring Material3d β‰₯30 MPa / 7d β‰₯40 MPa / 28d β‰₯50 MPaGB 50728‑2011Adhesive or cementitious anchorage in concrete
Explosion-proof / special floorsExplosion-Proof Concrete>140 MPaGB/T 39147-2020Anti-static and spark-resistant industrial floors
Waterproofing and insulationPolymer Cement Waterproof Mortarβ‰₯24.0 MPaJC/T 984‑2011Wet areas, basements and exterior insulation systems

2. Product quick reference

Grouting materials

ProductKey indicatorValueStandard
H60 Bearing Grouting MaterialCompressive Strength (28 Days)β‰₯60 MPa (25℃ curing)JC/T 986-2018
Cement Pavement Repair MaterialCompressive Strength1d β‰₯25 MPa / 3d β‰₯40 MPa / 28d β‰₯50 MPaJT/T 1124-2017
Explosion-Proof ConcreteCompressive Strength (28 Days)>140 MPaGB/T 39147-2020
High Strength Non-Shrink Grouting MaterialCompressive Strength1d β‰₯20 MPa / 3d β‰₯40 MPa / 28d β‰₯60 MPaGB/T 50448-2015
Prestressed Duct Grouting MaterialCompressive Strength3d β‰₯20 MPa / 7d β‰₯40 MPa / 28d β‰₯50 MPaJTG/T F50-2011
Rebar Anchoring MaterialCompressive Strength3d β‰₯30 MPa / 7d β‰₯40 MPa / 28d β‰₯50 MPaGB 50728‑2011
Sleeve Grouting MaterialCompressive Strength (28d)β‰₯85 MPaJG/T 408-2019
Tunnel Vault Grouting MaterialCompressive Strength (28d)β‰₯60 MPaGB/T 50448‑2015
Underwater Non-Dispersible Grouting MaterialCompressive Strength (28d)50–90 MPa (depending on class)GB/T 50448‑2015
Wind Turbine Foundation Grouting MaterialCompressive Strength (28d)>100 MPaGB/T 50448‑2015

Speciality cements

ProductKey indicatorValueStandard
Acid Resistant CementCompressive Strength (28d)β‰₯43.4 MPaGB/T 23456‑2018
Aluminate Cement24h Compressive Strength50–75 MPaGB/T 201-2015
Colored CementCompressive Strength (28d)β‰₯42.5 MPaGB/T 175-2023
Low Heat Expansion CementCompressive Strengthβ‰₯32.5 MPaGB 2938‑2008
Ordinary Portland CementCompressive Strength (28d)49.3 MPaGB 175‑2023
Rapid Hardening Sulphoaluminate Cement28d Compressive Strengthβ‰₯45.0 MPaGB/T 20472‑2006
White Portland CementCompressive Strength (28d)β‰₯42.5 MPaGB/T 2015‑2017

Polymer mortars

ProductKey indicatorValueStandard
AAC Block Masonry MortarCompressive Strengthβ‰₯5.0 MPa (depending on grade)JC/T 890-2017
Anti-Static Cement MortarCompressive Strength (28d)β‰₯25.0 MPaSJ/T 11294‑2018
Barium Sulfate Radiation Shielding MortarCube Compressive Strength (28d)β‰₯20.0 MPaJC/T 2676‑2022
Colored Cement Self-Leveling MortarCompressive Strength (28d)β‰₯42.5 MPaGB/T 1346
Polymer Cement Waterproof MortarCompressive Strength (28d)β‰₯24.0 MPaJC/T 984‑2011
Theme Park Sculpture MortarCompressive Strength (28d)β‰₯25.0 MPaJGJ/T 70‑2009
Thermal Insulation MortarCompressive Strengthβ‰₯0.50 MPaGB/T 20473‑2021

3. Five-step selection process

  1. 1
    Define the service condition

    Load type (static, dynamic, fatigue), temperature range, wet or dry exposure, and whether the grout is placed in a confined space.

  2. 2
    Set the strength requirement at the commissioning age

    A grout reaching 80 MPa at 28 days may still be unsuitable if the equipment must run at 3 days. Specify the age, not just the number.

  3. 3
    Match flowability to the placement method

    Thin layers and long flow paths need higher flow; large volumes and deep pours need a mix that does not segregate.

  4. 4
    Confirm the standard and test report

    Chinese cementitious grouts are commonly tested to GB/T 50448-2015; sleeve grouting to JG/T 408-2019. Ask for a batch test report.

  5. 5
    Run a trial batch for critical work

    For anchor bolts, bearings and turbine connections, place a trial section and verify flow, set time and strength before the main pour.

Need help with a specific condition?

Send the load, temperature and placement details and we will recommend a mix and test plan.

Contact our team